Hematite
Ground natural iron(III) oxide ore with a specific gravity of about 4.9. It reaches high slurry and fluid densities at lower solids loading than barite, keeping rheology manageable in heavy-weight designs. Its main use is weighting oil-well cement slurries for high-pressure zones (2.30 g/cm³ and above); it is also used to weight drilling and completion fluids. Chemically inert, thermally stable and compatible with common cementing additive systems.
Specification
| Property | Value |
|---|---|
| Product characteristics | |
| Appearance | Dark red-brown to black fine powder |
| Principal constituent | Hematite (iron(III) oxide, Fe₂O₃) |
| Specific gravity, g/cm³ | ≈ 4.9 |
| Solubility in water | Practically insoluble; chemically inert in slurry |
| Grind | Fine powder — cementing weighting grade |
| Verified slurry performance — Class G cement, laboratory test | |
| Hematite concentration | 75 % BWOC |
| Slurry density achieved | 2.350 g/mL (19.61 ppg) |
| Slurry yield | 99.22 L / 100 kg |
| Mix water | 52.17 L / 100 kg |
| Free fluid | 0.0 mL (0 %) |
| Test conditions | BHCT 65 °C · BHP 64 MPa · time to bottom 50 min |
Application & dosage
In cementing, typically 40 – 100 % BWOC to reach densities of 2.2 – 2.4 g/cm³ and above, together with dispersant and fluid-loss control per the laboratory design. Dry-blend with cement or add through the mixing system with adequate shear. In drilling fluids, add through the hopper as with barite; hematite is harder and more abrasive, so monitor pump and equipment wear.